LumberLay
Meet our LumberLay filaments – a unique material that has the look and feel of real wood. LumberLay combines 40% of recycled wood and 60% of PLA filament. Because of this mix, your prints will have the appearance of natural wood, and the physical properties of the product will be extremely similar to natural wood.
Please note: The LumberLay filaments must be dried before use (8 hours at 55°C) and are not compatible with a 0.2 mm nozzle.
LumberLay Pine Sample
Experiment with our LumberLay Pine sample and let the fun begin.
To know more about LumberLay filaments, read our blog.
You can access the Technical Data Sheet here.
Printing recommendations:
- The filament must be dried before use (8 hours at 55°C).
- LumberLay filaments are not compatible with a 0.2 mm nozzle.
- For the best results, print at 200–230°C.
- Recommended printing table temperature is 60°C.
- Use a glass bed, PEI sheet, Kapton, or Blue tape for the build platform with 3Dlac spray.
*Ideal temperature may vary when using different printers.